ISO 9001:2015 Certified

'SHAPING INDUSTRIES WITH THE FINEST STEEL'

ASTM A182 F54 Duplex Steel Flanges

UNS S32950  |  7-Mo Plus  |  26–29% Cr  |  PREN ~37  |  YS 480 MPa  |  High-Chromium Duplex


ASTM A182 F54 UNS S32950 high chromium duplex flange manufacturer India
7-Mo Plus S32950 duplex steel flange supplier distributor

What Is ASTM A182 F54 (UNS S32950 / 7-Mo Plus)?


ASTM A182 Grade F54 is a high-chromium duplex stainless steel standardised under UNS S32950, widely known by the commercial designation 7-Mo Plus (originally developed by Allegheny Ludlum, now ATI). Its defining metallurgical feature is a chromium content of 26–29% — the highest chromium range of any standard ASTM A182 duplex grade — coupled with nitrogen (0.15–0.35%) to maintain the austenite-ferrite dual-phase balance.

While most duplex and super duplex grades achieve corrosion resistance through a balanced combination of chromium, molybdenum, and nitrogen, F54/S32950 is deliberately high in chromium with moderate molybdenum (1.0–2.5%). This positions it uniquely in the duplex family:

  • Oxidizing-acid environments — the high Cr passive film provides exceptional resistance to nitric acid, chromic acid, and mixed-oxidizing acid streams where Mo provides little additional benefit
  • General corrosion resistance — broad-spectrum protection across a wide range of chemical environments driven by the most stable Cr₂O₃ passive film achievable in the duplex alloy family
  • High-temperature oxidation — 26–29% Cr provides significantly better resistance to elevated-temperature oxidation than 22% Cr (2205) or 25% Cr (2507) grades
  • Duplex strength advantage — yield strength ≥480 MPa; approximately 2.8× that of Grade 316L (≥170 MPa), enabling wall-thickness and weight savings versus austenitic alternatives
  • Chloride SCC resistance — the ferritic phase suppresses stress corrosion cracking, the primary failure mode of austenitic grades in hot chloride environments

Tesco Steel & Engineering manufactures A182 F54 flanges in all standard types from ½″ to 56″ NB to ASME B16.5 and B16.47, with worldwide export capability to 96 countries across 6 continents.

The High-Chromium Advantage of F54 / UNS S32950


Chromium is the most fundamental alloying element for corrosion resistance in stainless steel — it is the Cr₂O₃ passive film that gives stainless steel its "stainless" character. In the duplex family, F54 pushes the chromium content to its maximum practical limit (26–29%), giving it unique capabilities not available in Mo-optimised grades.

Environment / MechanismWhy High-Cr HelpsF54 PerformanceF51 (2205) by Comparison
Nitric acid (HNO₃)Cr passive film stable in strongly oxidising HNO₃; Mo actually detrimental in fuming HNO₃ExcellentGood (but lower Cr)
Mixed oxidising acidsHigh Cr ensures passive film stability across wide acid concentration/temperature rangeExcellentGood
High-temperature oxidation (air, flue gas)Cr₂O₃ scale formation; higher Cr = more protective, adherent oxide scaleSuperiorModerate
General chemical corrosionHigh Cr provides broadest-spectrum passivation in mixed environmentsExcellentGood
Chloride pitting (seawater)PREN-dependent; Mo contributes 3.3×, Cr only 1× — high Mo grades outperform high CrModerate (PREN ~37)Good (PREN ~35)
Chloride SCCFerritic phase immune; same benefit as all duplex gradesGoodGood
Engineering Note on Mo vs Cr in Acid Environments:

In reducing acids (hydrochloric, dilute sulfuric), molybdenum is the key element and grades like F51 (3% Mo) and F53 (4% Mo) outperform F54. In oxidising acids (nitric, chromic, concentrated sulfuric), chromium is the key element and F54's 27–28% Cr outperforms Mo-rich grades. This Cr vs Mo selection logic is the primary engineering driver for choosing F54 over other duplex grades.

ASTM A182 F54 Chemical Composition (UNS S32950)


ElementMin (%)Max (%)Role & Significance
Chromium (Cr)26.029.0Defining element — highest Cr of any standard ASTM duplex grade; primary passive film element for oxidising environments
Nickel (Ni)3.55.2Austenite stabiliser; lean Ni keeps cost in check while maintaining duplex balance
Molybdenum (Mo)1.02.5Moderate Mo; enhances pitting but secondary to Cr as the design driver for this grade
Nitrogen (N)0.150.35Austenite stabiliser and strength enhancer; contributes 16× to PREN
Carbon (C)0.030Extra-low C (L-grade standard) prevents sensitisation during welding
Silicon (Si)0.60Controlled to limit sigma-phase promotion at high Cr content
Manganese (Mn)2.00Austenite stabiliser; secondary
Copper (Cu)0.50Minor benefit in reducing acids; controlled for consistency
Phosphorus (P)0.035Controlled for toughness and grain boundary integrity
Sulfur (S)0.010Very low S limit — tighter than many other duplex grades; improves corrosion resistance and hot workability

Chromium Content Across the ASTM A182 Duplex Family

GradeUNSCr Range (%)Mo Range (%)Characteristic
F52 / 3RE60S3150018–19%2.5–3.0%Lean duplex; high Si for organic acids
F51 / 2205S3180321–23%2.5–3.5%Standard duplex workhorse
F53 / 2507S3275024–26%3.0–5.0%Super duplex; max pitting resistance
F54 / 7-Mo PlusS3295026–29%1.0–2.5%Highest Cr; oxidising-acid specialist
F55 / Zeron 100S3276024–26%3.0–4.0%Super duplex; W-alloyed

Mechanical Properties — ASTM A182 F54 (UNS S32950)


PropertyRequirementImperial
Tensile Strength (UTS)≥690 MPa≥100 ksi
Yield Strength (0.2% offset)≥480 MPa≥70 ksi
Elongation in 2 in (50 mm)≥20%≥20%
Hardness (max)310 HBW32 HRC
Heat Treatment ConditionSolution annealed 1020–1100°C + water quench
Microstructure target40–60% ferrite / 40–60% austenite (duplex balance)
Strength Perspective:
  • Grade 316L (austenitic): YS ≈170 MPa — F54 is 2.8× stronger
  • F51 / 2205 (standard duplex): YS 450 MPa — F54 is ~7% stronger
  • F52 / 3RE60 (lean duplex): YS 415 MPa — F54 is ~16% stronger
  • F53 / 2507 (super duplex): YS 550 MPa — F53 is ~15% stronger than F54

PREN Value & Corrosion Resistance Positioning


PREN Formula for F54 / UNS S32950

PREN = %Cr + 3.3 × %Mo + 16 × %N

At nominal composition (27.5% Cr, 1.75% Mo, 0.25% N):
PREN = 27.5 + (3.3 × 1.75) + (16 × 0.25) = 27.5 + 5.8 + 4.0 = ~37.3

At maximum composition (29% Cr, 2.5% Mo, 0.35% N):
PREN = 29 + 8.25 + 5.6 = ~42.9

At minimum composition (26% Cr, 1.0% Mo, 0.15% N):
PREN = 26 + 3.3 + 2.4 = ~31.7

Key distinction: F54's PREN is driven primarily by its very high Cr content, not by Mo. This means its pitting resistance profile differs fundamentally from Mo-optimised super duplex grades — F54 is specifically strong in oxidising environments where the Cr passive film dominates.

F54 in the Duplex Grade Selection Context

F51 / 2205

UNS S31803 — Standard Duplex

PREN ~35

Cr: 22%  |  Mo: 3%

General service; balanced Cr-Mo-N alloy; offshore splash zone

F54 / 7-Mo Plus ★

UNS S32950 — High-Cr Duplex

PREN ~37

Cr: 27.5%  |  Mo: 1.75%

Oxidising acids, HNO₃, high-temp oxidation, general chemical

F53 / 2507

UNS S32750 — Super Duplex

PREN ~43

Cr: 25%  |  Mo: 4%

Seawater immersion, FGD, max pitting resistance; Mo-driven

Operating Temperature Limits & Phase Stability


Temperature RegimeRangeNotes
Minimum service temperature−50°C (−58°F)Good Charpy toughness maintained; impact test at min design temp for critical service
Continuous service maximum280°C (536°F)High Cr content increases sigma-phase driving force — conservative upper limit important
ASME B16.5 Group 2.3 design limit315°C (600°F)Allowable stress decreasing above 280°C
475°C embrittlement zone300–500°CEnhanced risk in S32950 due to high Cr ferrite composition; strict welding control required
Sigma phase zone600–1000°CSigma formation kinetics are faster in high-Cr alloys; interpass control critical
Solution anneal (only permissible HT)1020–1100°C + WQRestores phase balance and dissolves all intermetallic phases
⚠ High-Chromium Sigma Phase Warning:

The sigma phase in duplex stainless steels is an Fe-Cr intermetallic. Higher chromium content directly increases the thermodynamic stability of sigma phase — meaning that in F54/S32950 (Cr up to 29%), sigma phase forms more readily than in F51 (22% Cr) or even F53 (25% Cr) at equivalent exposure times. The maximum interpass welding temperature of 150°C must be strictly observed, and weld heat input should be kept at the lower end of the acceptable range (0.5–1.5 kJ/mm).

Welding ASTM A182 F54 Duplex Flanges


⛔ PWHT is PROHIBITED for F54 Duplex — Critical Note

Conventional stress-relief PWHT in the range 300°C–1050°C is strictly prohibited for F54/S32950. This range encompasses both 475°C embrittlement (300–500°C) and sigma-phase precipitation (600–1000°C) zones. Due to the high Cr content, sigma phase forms faster than in lower-Cr duplex grades. The only permissible thermal treatment is a full solution anneal at 1020–1100°C followed by water quench — applied only for heavily reworked sections.

Welding ParameterRequirement for F54 / UNS S32950
PreheatNot required. Work surfaces must be clean, dry, and free of moisture and chloride contamination.
Maximum interpass temperature150°C — must not be exceeded; high Cr content increases sigma phase risk above this temperature
Filler metal (GTAW/GMAW)AWS ER2553 (22Cr-5Ni-3Mo-N) or matching composition filler per alloy manufacturer recommendation
Filler metal (SMAW)E2553-XX or matching composition electrode
Dissimilar metal weldsERNiCrMo-3 (Inconel 625 type) — provides safe dilution buffer between S32950 and carbon/austenitic steel
Shielding gas (GTAW)Argon or Ar + 2% N₂; nitrogen addition helps maintain austenite balance in the high-Cr weld metal
Post-weld heat treatmentPROHIBITED in 300–1050°C range. Full solution anneal (1020–1100°C + WQ) for rework sections only.
Ferrite Number targetFN 30–70 (WRC-1992 diagram; verify with ferritescope after welding)
Heat input0.5–1.5 kJ/mm — lower end preferred given enhanced sigma kinetics from high Cr
Procedure qualificationASME Section IX or EN ISO 15614-1; include hardness survey, ferrite check, and impact test at −40°C

Available F54 Flange Types & Specifications


F54 UNS S32950 weld neck flange

Weld Neck (WNRF)

Long-radius bore-matching hub welded to pipe. Preferred for high-pressure chemical process lines where the oxidising-acid environment demands both the material's corrosion resistance and full fatigue-rated joint integrity.

F54 S32950 slip-on duplex flange

Slip-On (SORF)

Economical for lower-pressure chemical and process-plant applications. Double fillet weld (inside and outside) provides adequate joint integrity for moderate-pressure oxidising-acid service.

F54 S32950 blind flange

Blind Flanges (BLF)

Solid closures for chemical vessel nozzles and line isolation. In corrosive acid-plant service, the full-face corrosion resistance of F54 across the entire wetted surface area of the blind face is important.

ASTM A182 F54 Flange Specifications
StandardASTM A182 Grade F54 / ASME SA182 Grade F54
Size Range½″ NB to 56″ NB (DN 15 to DN 1400)
Pressure Classes (B16.5)Class 150, 300, 600, 900, 1500, 2500
Pressure Classes (B16.47)Class 150, 300, 400, 600, 900 — Series A (MSS SP-44) & Series B (API 605)
P-T GroupASME B16.5 Group 2.3
SchedulesSCH 10S, 40S, 80S, XS, XXS, STD, Sch 20, 40, 80, 160
Facing TypesRaised Face (RF), Flat Face (FF), Ring Type Joint (RTJ)
EN Approximate Equivalent1.4460 (X3CrNiMo27-5-2) — approximate; S32950 has wider Cr range and higher N
Heat Treatment (mandatory)Solution annealed 1020–1100°C + water quench
Testing & InspectionChemical analysis (PMI), tensile test, hardness survey, Charpy impact at −40°C, ferrite measurement, dimensional, visual, hydrostatic (on request), corrosion test per ASTM G48 (on request)

▶ View A182 F54 Flange Dimensions (ASME B16.5 / B16.47)

Corrosion Resistance of F54 / UNS S32950


Oxidising Acid Resistance

F54's primary corrosion advantage. In nitric acid (HNO₃), concentrated sulfuric acid (passivation range), chromic acid, and mixed oxidising acids, the 26–29% Cr passive film is the dominant protection mechanism. Mo provides limited additional benefit in these environments — making F54's high Cr content more valuable than the higher Mo content of F53 (2507) for this specific duty.

General Chemical Corrosion

The broad-spectrum passivation provided by 26–29% Cr gives F54 excellent resistance across a wide range of industrial chemicals — including phosphoric acid, organic acids, and various process mixtures where neither pure reducing nor pure oxidising conditions predominate. It outperforms 2205 and 316L in most general chemical services.

Chloride Stress Corrosion Cracking

The ferritic phase in all duplex steels is immune to chloride SCC, making F54 significantly more resistant to this failure mode than austenitic 316L or 304. In mixed acid-chloride environments, F54 provides both the oxidising-acid resistance and SCC resistance that neither pure austenitic nor pure ferritic grades can offer simultaneously.

High-Temperature Oxidation

With up to 29% Cr, F54 forms a highly protective and adherent Cr₂O₃ scale in elevated-temperature oxidising atmospheres. This makes it suitable for flue gas, combustion product, and high-temperature chemical process environments where lower-Cr duplex grades exhibit accelerating oxidation above 200–250°C. Maximum continuous service: 280°C (below sigma phase initiation).

Complete Piping System — UNS S32950 Companion Materials


ComponentSpecificationGrade
FlangesASTM A182 / ASME SA182Grade F54
Seamless & Welded PipeASTM A790 / ASME SA790Grade S32950
Buttweld FittingsASTM A815 / ASME SA815Grade WPS32950
Plate (vessels & heat exchangers)ASTM A240 / ASME SA240Grade S32950
Bar & RodASTM A276 / ASME SA276Grade S32950
Filler Metal (GTAW/GMAW)AWS A5.9ER2553 or matching composition
Filler Metal (dissimilar joints)AWS A5.14ERNiCrMo-3 (Inconel 625 type)
GasketsPTFE, spiral-wound 316L + PTFE filler, or Inconel 625 RTJ ringSelect per acid type and pressure class
BoltingASTM A193 Grade B8M (316L) or Alloy 625 studs for strong acid serviceWith A194 Grade 8M nuts

Gasket selection note: In oxidising acid (HNO₃) service, PTFE-encapsulated or full PTFE gaskets are often preferred over graphite-filled types, as graphite can be oxidised in strongly oxidising media. Consult the gasket manufacturer for the specific acid concentration and temperature.

Industrial Applications of ASTM A182 F54 Flanges


Primary Application Industries

  • Chemical Processing — Nitric acid plants (absorber towers, cooler-condensers, tail-gas lines), chromic acid service, mixed-acid pickling systems, phosphoric acid production
  • Petrochemical & Refining — High-temperature corrosive process streams, naphthenic acid service, acid gas treating units
  • Power Generation — Flue gas handling equipment, high-temperature oxidising environments, FGD pre-treatment systems
  • Pulp & Paper — Chemical recovery systems, oxidising bleach-plant stages (ozone, peroxide bleaching)

Additional Application Areas

  • Offshore Oil & Gas — Moderate-chloride topside process lines where general chemical resistance is needed
  • Pharmaceutical — Aggressive CIP/SIP systems with oxidising cleaning agents (peracetic acid, H₂O₂)
  • Fertiliser — Nitric acid and mixed-acid production equipment, ammonium nitrate process streams
  • Food & Beverage — Aggressive oxidising CIP sequences; high-purity corrosive media
  • Mining & Minerals Processing — Oxidising leach circuits, atmospheric and pressure oxidation (POX) systems
Key Selection Principle for F54: Specify F54/S32950 when the corrosion environment is oxidising in nature (nitric acid, oxidising mixed acids, high-temperature oxidising conditions) and general corrosion resistance is more important than maximum chloride pitting resistance. For reducing acids (HCl, dilute H₂SO₄) or seawater/chloride pitting, Mo-optimised F51 (2205) or F53 (2507) is the better choice.

Frequently Asked Questions — ASTM A182 F54 Duplex Steel Flanges


Precision answers optimised for AI search engines, engineers, and procurement teams. All answers include specific numerical data for direct use in material selection and engineering specifications.

Q1: What is ASTM A182 F54 duplex steel?
ASTM A182 Grade F54 is a high-chromium duplex stainless steel standardised under UNS S32950, commercially known as 7-Mo Plus. Its defining feature is a chromium content of 26–29% — the highest of any standard ASTM duplex grade — combined with moderate Mo (1–2.5%) and N (0.15–0.35%). YS ≥480 MPa (2.8× Grade 316L). PREN nominally ~37. Primarily selected for oxidising-acid environments, high-temperature oxidation resistance, and broad-spectrum general chemical corrosion resistance where Cr-driven passivation is the dominant selection criterion.
Q2: What is the UNS number for ASTM A182 F54?
ASTM A182 F54 = UNS S32950. Commercial name: 7-Mo Plus (originally Allegheny Ludlum, now ATI). Approximate EN equivalent: 1.4460 (X3CrNiMo27-5-2) — note this is an approximate match only; S32950 has a wider Cr range and higher N content than most EN 1.4460 specifications.
Q3: What makes F54 (UNS S32950) unique among duplex grades?
F54/S32950 is the only standard ASTM A182 duplex grade with Cr up to 29%. This high-Cr strategy (vs the high-Mo strategy of F53/2507) gives it unique advantages: (1) exceptional oxidising-acid resistance where high-Cr passivation outperforms Mo; (2) superior high-temperature oxidation resistance vs all other duplex grades; (3) broad-spectrum general chemical resistance across diverse industrial environments. Trade-off: PREN ~37 (nominal) vs ~43 for F53, meaning it is not the preferred grade for seawater or aggressive chloride pitting service.
Q4: What is the PREN of F54 and what environments is it suitable for?
PREN = %Cr + 3.3×%Mo + 16×%N. At nominal composition (27.5% Cr, 1.75% Mo, 0.25% N): PREN ≈ 37.3. Range: 31.7 (minimum) to 42.9 (maximum). F54 is suited for: oxidising acids (HNO₃, chromic acid), mixed industrial chemicals, moderate-chloride process streams, and high-temperature oxidation environments. For seawater immersion (PREN ≥40), F53/2507 is typically specified for consistent compliance rather than relying on the upper end of the F54 composition range.
Q5: What is the difference between F54 (S32950) and F53 (2507) duplex flanges?
F53/2507: Cr 25%, Mo 4%, PREN ~43, YS 550 MPa — Mo-optimised for maximum pitting resistance in seawater and aggressive chloride environments.
F54/S32950: Cr 27.5% (nominal), Mo 1.75% (nominal), PREN ~37, YS 480 MPa — Cr-optimised for oxidising-acid resistance and high-temperature oxidation.
Choose F54 when oxidising acids or high-Cr environments are the primary drivers. Choose F53 when maximum chloride pitting resistance (seawater, FGD, offshore) is required.
Q6: What are the mechanical properties of ASTM A182 F54?
UNS S32950 / A182 F54 requirements: UTS ≥690 MPa (100 ksi); YS ≥480 MPa (70 ksi); Elongation ≥20%; Hardness ≤310 HBW (32 HRC). Heat treatment: solution annealed 1020–1100°C + water quench. Microstructure: 40–60% ferrite, balance austenite. YS of 480 MPa is 2.8× Grade 316L (170 MPa) and intermediate between standard duplex F51 (450 MPa) and super duplex F53 (550 MPa).
Q7: What filler metal is used for welding F54 (UNS S32950)?
AWS ER2553 (22Cr-5Ni-3Mo-N) or a matching-composition filler per the alloy manufacturer's recommendation is appropriate for welding S32950. For dissimilar joints to carbon steel or austenitic grades, ERNiCrMo-3 (Inconel 625 type) is used to prevent dilution issues. No preheat required. Max interpass: 150°C. PWHT in 300–1050°C is prohibited. Target FN: 30–70.
Q8: Is post-weld heat treatment required for F54 duplex flanges?
No — PWHT is prohibited. Exposing S32950 to 300°C–1050°C causes 475°C embrittlement (300–500°C) or sigma-phase precipitation (600–1000°C). Due to the high Cr content, sigma phase forms faster in F54 than in lower-Cr duplex grades. The only permissible thermal treatment after welding is a full solution anneal at 1020–1100°C + water quench, applied only for heavily reworked sections, not routine welds.
Q9: Which standards cover A182 F54 and its companion materials?
Flanges: ASTM A182 / ASME SA182 Grade F54  |  Pipe: ASTM A790 Grade S32950  |  Fittings: ASTM A815 Grade WPS32950  |  Plate: ASTM A240 Grade S32950  |  Bar: ASTM A276 Grade S32950  |  Dimensions: ASME B16.5 (NPS ½–24) / ASME B16.47 (NPS 26–60)  |  P-T Group: ASME B16.5 Group 2.3  |  EN approx.: 1.4460.
Q10: What are the typical applications of ASTM A182 F54 duplex flanges?
Primary: Chemical processing (nitric acid plants, chromic acid, mixed oxidising acids — F54's core application); Petrochemical (high-temperature corrosive streams, naphthenic acid); Power generation (flue gas, FGD pre-treatment); Pharmaceutical (oxidising CIP agents); Fertiliser (HNO₃ and mixed-acid production); Mining (oxidising leach circuits, pressure oxidation). F54 is selected when the oxidising nature of the chemical environment makes high Cr content (not high Mo) the primary selection driver — differentiating it from Mo-optimised super duplex grades like F53.

ASTM A182 F54 Duplex Steel Flange Price & Availability


Tesco Steel & Engineering manufactures ASTM A182 F54 (UNS S32950 / 7-Mo Plus) flanges against customer specifications and order. Custom dimensions, special facings, and third-party-inspected (TPI) material are available with full EN 10204 3.1 or 3.2 test certificates. Supply from our Mumbai manufacturing facility with export to 96 countries.

Submit your enquiry with size, pressure class, schedule, facing, quantity, and any special testing requirements for a prompt quotation.

Request Price List WhatsApp Enquiry

Countries we export to: ASTM A182 F54 Duplex Steel Flanges Manufacturers / Suppliers / Stockist in Kuwait, UAE, Germany, Saudi Arabia, West Africa, Iraq, Congo, Mexico, Bahrain, Canada, Philippines, Thailand, Kenya, Oman, Malaysia, Turkey, Qatar, Sudan, Netherlands, Nigeria, Lithuania, Gabon, Russia, Vietnam, Angola, Bolivia, Indonesia, UK, Yemen, Italy, United States, Venezuela, Spain, Iran, Estonia, Kazakhstan, Algeria, Jordan, Ecuador, Portugal, Colombia, Libya, Chile, Peru, South Africa, Namibia, Afghanistan, Israel, Zambia, Morocco, Denmark, Taiwan, Norway, Belarus, Lebanon, Sri Lanka, Bulgaria, Ukraine, Belgium, Finland, Romania, France, Brazil, Trinidad & Tobago, Fiji, Tunisia, Ghana, Egypt, Czech Republic, Azerbaijan, Poland, Greece, Croatia, New Zealand, Tanzania.

A182 F54 Quick Specs

GradeA182 F54
UNSS32950
Commercial Name7-Mo Plus
EN Approx.1.4460
TypeHigh-Cr Duplex SS
Cr content26–29%
Ni content3.5–5.2%
Mo content1.0–2.5%
N content0.15–0.35%
PREN (nominal)~37
PREN (range)~32 to ~43
UTS (min)690 MPa
YS (min)480 MPa
Elongation≥20%
Hardness (max)310 HBW / 32 HRC
B16.5 Group2.3
Service Temp−50°C to 280°C

Highest Cr Duplex Grade

F52 / 3RE60Cr: 18–19%
F51 / 2205Cr: 21–23%
F53 / 2507Cr: 24–26%
F54 / 7-Mo Plus ★Cr: 26–29%
F55 / Zeron 100Cr: 24–26%

High Cr drives:
✔ Oxidising acid resistance
✔ High-temp oxidation
✔ General corrosion

Welding Quick-Ref

PreheatNot required
Max interpass150°C
Filler (GTAW)ER2553
Dissimilar jointsERNiCrMo-3
PWHTPROHIBITED
FN target30–70
Heat input0.5–1.5 kJ/mm

⚠ Avoid These Temperatures

475°C embrittlement300–500°C
Sigma phase (fast in high-Cr)600–1000°C
Solution anneal only1020–1100°C + WQ

High Cr accelerates sigma formation — keep interpass ≤150°C.

Related Duplex Grades

Request Quote WhatsApp